https://doi.org/10.1051/epjconf/201715900043
The thermal expansion of hard magnetic materials of the Nd-Fe-B system
Kutateladze Institute of Thermal Physics, 630090 Novosibirsk, SB RAS, Russia
* Igor Savchenko: savchenko@itp.nsc.ru, savchenko.igor@gmail.com
Published online: 25 October 2017
The results of dilatometric measurement of the thermal expansion of hard magnetic materials brands N35M, N35H and N35SH containing as a main component the crystalline phase of Nd2Fe14B type are presented. The temperature range from 200 to 750 K has been investigated by the method of dilatometry with an error of 1.5-2×10-7 K-1. The approximation dependences of the linear thermal expansion coefficient have been obtained. The character of changes of the thermal coefficient of linear expansion in the region of the Curie point has been specified, its critical indices and critical amplitudes have been defined.
© The authors, published by EDP Sciences, 2017
This is an Open Access article distributed under the terms of the Creative Commons Attribution License 4.0, which permits unrestricted use, distribution, and reproduction in any medium, provided the original work is properly cited. (http://creativecommons.org/licenses/by/4.0/).